① STANDARD: EN10216-5/ASTM A312/ ASTM A249/ ASTM A269/ GOST 9940 /GOST 9941...② OD RANGE : 6-1016 MM③ THICKNESS RANGE: 1-65 MM
Grade |
C |
Mn |
P |
S |
Si |
Cr |
Ni |
Mo |
N |
Other |
316 |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1.00 |
16.00-18.00 |
10.00-14.00 |
2.00-3.00 |
– |
– |
316L |
≤0.035 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1.00 |
16.00-18.00 |
10.00-14.00 |
2.00-3.00 |
– |
– |
316H |
0.04-0.10 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1.00 |
16.00-18.00 |
11.00-14.00 |
2.00-3.00 |
– |
– |
316Ti |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤0.75 |
16.00-18.00 |
10.00-14.00 |
2.00-3.00 |
≤0.10 |
Ti:5×(C%+N)-0.7 |
316N |
≤0.08 |
≤2.00 |
≤0.045 |
≤0.03 |
≤1.00 |
16.00-18.00 |
10.00-14.00 |
2.00-3.00 |
0.10-0.16 |
– |
316LN |
≤0.035 |
≤2.00 |
≤0.045 |
≤0.015 |
≤1.00 |
16.00-18.00 |
10.00-14.000 |
2.00-2.50 |
0.10-0.16 |
– |
Grade |
Tensile Strength ksi(MPa) |
Yield Strength ksi(MPa) |
Elongation,% |
Hardness Brinell/Vickers |
Hardness Rockwell |
316 |
≥75(515) |
≥30(205) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316L |
≥70(485) |
≥25(170) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316H |
≥75(515) |
≥30(205) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316Ti |
≥75(515) |
≥30(205) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316N |
≥80(550) |
≥35(240) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316LN |
≥75(515) |
≥30(205) |
≥35 |
≤192HBW/200HV |
≤90HRB |
316Ti stainless steel pipes, also known as UNS S31635, find applications in various industries due to their unique properties. Let’s explore where they are commonly used:
Remember that 316Ti stainless steel combines strength, corrosion resistance, and versatility, making it valuable across diverse sectors!
Marked Pipe Sample: XTD ASTM A312 TP316Ti SEAMLESS 42.2x 3.56*6000MM HEAT NO. 2023121205A15
TP316Ti /1.4571/UNSS31635, is a titanium-stabilized, molybdenum-alloyed austenitic chromium-nickel steel with improved machinability has similar characteristics to AISI 316L, but the TP 316Ti has better mechanical properties and strength at high temperatures. TP 316Ti (1.4571, UNS S31635) due to the addition of titanium shows higher corrosion resistance.
TP 316Ti (1.4571, UNS S31635) is generally considered but is not resistant to hot sea water. Hot chloride environments may cause pitting and crevice corrosion. TP 316Ti (1.4571, UNS S31635) HEAT RESISTANCE 316 exhibits good resistance to oxidation in continuous service to a temperature of 870 ° C and a temperature of 925 ° C. However, if corrosion resistance to water is required, continuous use at 425-860 ° C is not recommended. In this case, 316L is recommended due to resistance to carbide precipitation. When high temperatures are required at temperatures above 500 ° C, class 316H is recommended.
① STANDARD: EN10216-5/ASTM A312/ ASTM A249/ ASTM A269/ GOST 9940 /GOST 9941...② OD RANGE : 6-1016 MM③ THICKNESS RANGE: 1-65 MM
① STANDARD: ASTM A312/ ASTM A249/ ASTM A269/ EN10216-5/GOST 9940 /GOST 9941...② OD RANGE : 6-1016 MM③ THICKNESS RANGE: 1-65 MM
① STANDARD: ASTM A213 A249,A267,A270,EN10216-5...② OD RANGE : 6-257MM③ THICKNESS RANGE: 1-35MM
① STANDARD: ASTM A213/ EN10216-5/ ASTM A249/ ASTM A269/ GOST 9940 /GOST 9941...② OD RANGE : 6-257MM③ THICKNESS RANGE: 1-35 MM
If you have any enquiry about quotation or cooperation,please feel free to email us at admin@xtd-ss.com or use the following enquiry form. Our sales will contact you within 24 hours. Thank you for your interest in our products.